Fractography is the study of the fracture surfaces of materials. Fractographic methods are routinely used to determine the cause of failure in engineering structures, especially in product failure and the practice of forensic engineering or failure analysis .
Fracture toughness varies by approximately 4 orders of magnitude across materials. Metals hold the highest values of fracture toughness. Cracks cannot easily propagate in tough materials, making metals highly resistant to cracking under stress and gives their stress–strain curve a large zone of plastic flow.
Polymer fracture is the study of the fracture surface of an already failed material to determine the method of crack formation and extension in polymers both fiber reinforced and otherwise. [1]
The impact energy of low-strength metals that do not show a change of fracture mode with temperature, is usually high and insensitive to temperature. For these reasons, impact tests are not widely used for assessing the fracture-resistance of low-strength materials whose fracture modes remain unchanged with temperature.
Fractured products can be examined using fractography, an especially useful method for all fractured components using macrophotography and optical microscopy. Although polymers usually possess quite different properties to metals and ceramics, they are just as susceptible to failure from mechanical overload , fatigue and stress corrosion ...
One place where you can do this is the popular ‘Google Earth, Structures and Anomalies’ group on Fa 50 Times People Found Such Strange Things On Google Earth, They Had To Share Them (New Pics ...
The next step would be to do an initial incident appraisal, this is done before any analysis is done and they take a quick observation of what the solution is at hand. [4] The third step in the investigative process is to plan how to the investigation will go and would resources they will need to obtain to do the analysis accurately. [ 4 ]
(Reuters) - Location tracking company Unacast has confirmed to the Norwegian government that it was the victim of a hack, according to a notice published by Norwegian public broadcaster NRK on Friday.