When testing wood in lumber form, the Janka test is always carried out on wood from the tree trunk (known as the heartwood), and the standard sample (according to ASTM D143) is at 12% moisture content and clear of knots. [3] The hardness of wood varies with the direction of the wood grain. Testing on the surface of a plank, perpendicular to the ...
Lignum vitae is hard and durable, and is also the densest wood traded (average dried density: ~79 lb/ft 3 or ~1,260 kg/m 3); [4] it will easily sink in water. On the Janka scale of hardness, which measures hardness of woods, lignum vitae ranks highest of the trade woods, with a Janka hardness of 4,390 lbf (compared with Olneya at 3,260 lbf, [5] African blackwood at 2,940 lbf, hickory at 1,820 ...
Red oak rings in at a 1290 on the Janka scale (the higher the number, the stronger the board), and white oak comes in at 1360. Durability: Thanks to the wood’s open grain, wood stains take ...
Jeffrey pine wood and ponderosa pine wood are sold together as yellow pine. [6] Both kinds of wood are hard (with a Janka hardness of 550 lbf (2,400 N)), but the western yellow pine wood is less dense than southern yellow pine wood (28 lb/cu ft (0.45 g/cm 3 ) versus 35 lb/cu ft (0.56 g/cm 3 ) for shortleaf pine).
Ironwood is a common name for many woods that have a reputation for hardness, or specifically a wood density that is denser than water (approximately 1000 kg/m 3, or 62 pounds per cubic foot), although usage of the name ironwood in English may or may not indicate a tree that yields such heavy wood.
The wood is very hard, measuring 5.6 on the Brinell scale and 2,350 lbf (10,500 N) on the Janka scale, approximate measurements of hardness. For comparison, Douglas fir measures 660 lbf (2,900 N), white oak 1,360 lbf (6,000 N), and Brazilian walnut 3,800 lbf (17,000 N) on the Janka scale. It features a tan to salmon color with black accent ...
Towards the centre of the trunk, the wood gets less hard. The wood has a Janka ball hardness of 112.5 - 154.7 kgf/cm 2 (1600 – 2200 psi), which is greater than that of oak (70.3 - 84.4 kgf/cm 2) and Douglas fir (35.9 kgf/cm 2). Coconut timber is classified according to three degrees of density: High-density timber (dermal) – hard: 600–900 ...
Cocobolo is yielded by two to four closely related species of the genus Dalbergia, of which the best known is Dalbergia retusa, a fair-sized tree, reported to reach 75–80 ft (23–24 m) in height and 3 ft (0.9 m) in diameter; [1] it probably is the species contributing most of the wood in the trade.