904L is an austenitic stainless steel.It is softer than 316L, [1] [2] and its molybdenum addition gives it superior resistance to localized attack (pitting and crevice corrosion) by chlorides and greater resistance reducing acids; in particular, its copper addition gives it useful corrosion resistance to all concentrations of sulfuric acid.
Alloy 20 is an austenitic stainless steel containing less than 50% iron developed for applications involving sulfuric acid.Its corrosion resistance also finds other uses in the chemical, petrochemical, power generation, and plastics industries.
Green death is a solution used to test the resistance of metals and alloys to corrosion. It consists of a mixture of sulfuric acid, hydrochloric acid, iron(III) chloride and copper(II) chloride and its boiling point is at approximately 103 °C. Its typical chemical composition is given in the table hereafter: [1] [2] [3] [4]
For example, alloy 020 is designed to be resistant to sulfuric acid, and the DS Incoloy is to be used in heat-treating furnaces with reactive atmospheres and many heat cycles. Incoloy 020 "exhibits excellent corrosion resistance in chemical environments that contain sulfuric acid, chlorides, phosphoric acid and nitric acid." [5]
Stainless steel, also known as inox, corrosion-resistant steel (CRES), and rustless steel, is an iron-based alloy containing a minimum level of chromium that is resistant to rusting and corrosion. Stainless steel's resistance to corrosion results from the 10.5%, or more, chromium content which forms a passive film that can protect the material ...
Alloy 20 (Carpenter 20) is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would readily attack type 316 stainless. This alloy exhibits superior resistance to stress-corrosion cracking in boiling 20–40% sulfuric acid.
Sulfuric acid is a colorless oily liquid, and has a vapor pressure of <0.001 mmHg at 25 °C and 1 mmHg at 145.8 °C, [16] and 98% sulfuric acid has a vapor pressure of <1 mmHg at 40 °C. [ 17 ] In the solid state, sulfuric acid is a molecular solid that forms monoclinic crystals with nearly trigonal lattice parameters.
The lead chamber process for sulfuric acid production was abandoned, partly because it could not produce sulfur trioxide or concentrated sulfuric acid directly due to corrosion of the lead, and absorption of NO 2 gas. Until this process was made obsolete by the contact process, oleum had to be obtained through indirect methods. Historically ...