Search results
Results from the WOW.Com Content Network
Sinister 2 (stylized in marketing as Sinister II) is a 2015 supernatural horror film directed by Ciarán Foy, and written by Scott Derrickson and C. Robert Cargill. A sequel to Sinister (2012), it stars James Ransone , reprising his role from the original film, and Shannyn Sossamon .
Sintering or frittage is the process of compacting and forming a solid mass of material by pressure [1] or heat [2] without melting it to the point of liquefaction. Sintering happens as part of a manufacturing process used with metals , ceramics , plastics , and other materials.
Next, solvent is used to remove a portion of the binder material from the printed parts, leaving "brown" parts. Finally, after thermal debinding and sintering, near net-shape metal parts are produced. The system was announced in 2017 [26] and launched in 2018, consisting of the Metal X printer, Wash-1 debinding station, and Sinter-1 furnace ...
Sinter plant, in which iron-ore dust gets mixed with other fine materials at high temperature, to create a product – sinter – for use in a blast furnace; Sintering, a high temperature process for fusing powder together; Calcareous sinter, calcium carbonate deposited by springs; Siliceous sinter, silica deposited by hot springs and geysers
Schunk Sinter Metals primarily produces sintered structural parts such as gearwheels, camshaft adjusters, locking cams, metal injection mold (MIM) parts as well as precision bearings. The main users are in the automotive and electric industries, or are producers of household and power tools and medical technology.
An SLS machine being used at the Centro de Pesquisas Renato Archer in Brazil.. Selective laser sintering (SLS) is an additive manufacturing (AM) technique that uses a laser as the power and heat source to sinter powdered material (typically nylon or polyamide), aiming the laser automatically at points in space defined by a 3D model, binding the material together to create a solid structure.
Main feed into a sinter plant is base mix, which consists of iron ore fines, coke fines and flux (limestone) fines. In addition to base mix, coke fines, flux fines, sinter fines, iron dust (collected from plant de-dusting system and electrostatic precipitator) and plant waste are mixed in proportion (by weight) in a rotary drum, often called mixing and nodulizing drum.
Sinter plate filter elements were developed in Germany [6] during the years of 1981 and 1982. These rigid filter elements are used in dust collectors and will produce clean gas values of 0.1 to 1.0 mg/m 3 with emissions of 0.001 pounds per hour with a maximum of 0.0004 gr/ft3, even with dusts of D50 < 1 μm.