Search results
Results from the WOW.Com Content Network
2024-O temper aluminium has no heat treating. It has an ultimate tensile strength of 140–210 MPa (21–30 ksi), and a maximum yield strength of no more than 97 MPa (14,000 psi). The material has elongation (stretch before ultimate failure) of 10–25%, this is the allowable range per applicable AMS specifications.
The alloy and its various tempers are covered by the following standards: [2] ASTM B 221: Standard Specification for Aluminum and Aluminum-Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes; EN 573-3: Aluminium and aluminium alloys. Chemical composition and form of wrought products. Chemical composition and form of products
A UNS number only defines a specific chemical composition, it does not provided full material specification. Requirements such as material properties (yield strength, ultimate strength, hardness, etc.), heat treatment, form (rolled, cast, forged, flanges, tubes, bars, etc.), purpose (high temperature, boilers and pressure vessels, etc.) and testing methods are all specified in the material or ...
9 Aluminum alloy table. ... Download as PDF; Printable version; In other projects ... This page was last edited on 9 May 2024, at 18:51 (UTC).
6082 aluminium alloy is an alloy in the wrought aluminium-magnesium-silicon family (6000 or 6xxx series). It is one of the more popular alloys in its series (alongside alloys 6005, 6061, and 6063), although it is not strongly featured in ASTM (North American) standards.
7068 alloy is a 7000 series aluminium-zinc alloy registered with the US Aluminium Association and produced to AMS 4331 (chemical composition and mechanical properties) and AMS 2772 (heat treatment). 7068 alloy ‘A’ and ‘B’ tensile data and fatigue properties have been ratified for inclusion in MIL Handbook 5 / MMPDS.
EN 1090-1 : Execution of steel structures and aluminium structures – Part 1 : General technical delivery conditions for structural steel and aluminium components; EN 1090-3 : Execution of steel structures and aluminium structures – Part 3 : Technical requirements for aluminium structures. Eurocode 9 has five parts: [1]
Print/export Download as PDF; Printable version; In other projects Wikidata item; Appearance. ... Aluminum: ≥ 99.7 Iron: ≤ 0.25 Silicon: ≤ 0.20 Zinc: