A common use of Janka hardness ratings is to determine whether a species is suitable for use as flooring. For hardwood flooring, the test usually requires an 80 mm × 150 mm (3 in × 6 in) sample with a thickness of at least 6–8 mm, and the most commonly used test is the ASTM D1037.
Lignum vitae is hard and durable, and is also the densest wood traded (average dried density: ~79 lb/ft 3 or ~1,260 kg/m 3); [4] it will easily sink in water. On the Janka scale of hardness, which measures hardness of woods, lignum vitae ranks highest of the trade woods, with a Janka hardness of 4,390 lbf (compared with Olneya at 3,260 lbf, [5] African blackwood at 2,940 lbf, hickory at 1,820 ...
The wood from A. peregrina produces very hard timber that is used for making furniture. [7] It has a Janka rating of 3700 lb. [8] [failed verification] and a density of around 0.86 g/cm 3. [9] Tannins have also been derived from this plant. [4]
Jeffrey pine wood and ponderosa pine wood are sold together as yellow pine. [6] Both kinds of wood are hard (with a Janka hardness of 550 lbf (2,400 N)), but the western yellow pine wood is less dense than southern yellow pine wood (28 lb/cu ft (0.45 g/cm 3 ) versus 35 lb/cu ft (0.56 g/cm 3 ) for shortleaf pine).
NCSU Inside Wood project; Reproduction of The American Woods: exhibited by actual specimens and with copious explanatory text by Romeyn B. Hough; US Forest Products Laboratory, "Characteristics and Availability of Commercially Important Wood" from the Wood Handbook Archived 2021-01-18 at the Wayback Machine PDF 916K; International Wood ...
The wood is very hard, measuring 5.6 on the Brinell scale and 2,350 lbf (10,500 N) on the Janka scale, approximate measurements of hardness. For comparison, Douglas fir measures 660 lbf (2,900 N), white oak 1,360 lbf (6,000 N), and Brazilian walnut 3,800 lbf (17,000 N) on the Janka scale. It features a tan to salmon color with black accent ...
The name sapele comes from that of the city of Sapele in Nigeria, where there is a preponderance of the tree.African Timber and Plywood (AT&P), a division of the United Africa Company, had a factory at this location where the wood, along with Triplochiton scleroxylon, Obeche, mahogany, and Khaya was processed into timber which was then exported from the Port of Sapele worldwide.
Moisture content of dried wood: 12 per cent; Density of wood: 560 kg/m 3; Tensile strength: 88 MPa; Modulus of elasticity: 9.1 GPa; After felled kauri wood dries to a 12 per cent moisture content, the tangential contraction is 4.1 per cent and the radial contraction is 2.3 per cent. Kauri is considered a first rate timber.