Search results
Results from the WOW.Com Content Network
Nickel-based superalloys are used in load-bearing structures requiring the highest homologous temperature of any common alloy system (Tm = 0.9, or 90% of their melting point). Among the most demanding applications for a structural material are those in the hot sections of turbine engines (e.g. turbine blade). They comprise over 50% of the ...
[4] [5] Nimonic 80a was used for the turbine blades on the Rolls-Royce Nene and de Havilland Ghost, Nimonic 90 on the Bristol Proteus, and Nimonic 105 on the Rolls-Royce Spey aviation gas turbines. Nimonic 263 was used in the combustion chambers of the Rolls-Royce/Snecma Olympus 593 used on the Concorde supersonic airliner. The heads of the ...
Waspaloy is an age-hardenable, nickel-based superalloy with excellent strength properties through temperatures of roughly 980°C (1800°F). Other characteristics of Waspaloy include good corrosion resistance, as well as being relatively impervious to oxidation making it well suited for service in extreme environments.
Inconel 713C: Precipitation hardenable nickel-chromium base cast alloy [2] Inconel 718: Gamma double prime strengthened with good weldability [72] Inconel 738; Inconel X-750: Commonly used for gas turbine components, including blades, seals and rotors. Inconel 751: Increased aluminum content for improved rupture strength in the 1600 °F range [73]
The turbine blades are often the limiting component of gas turbines. [4] To survive in this difficult environment, turbine blades often use exotic materials like superalloys and many different methods of cooling that can be categorized as internal and external cooling, [5] [6] [7] and thermal barrier coatings.
The nickel-based superalloys are well known for their intensive use in the industrial field especially the aeronautical and the aerospace industry due to their superior mechanical and corrosion properties at high temperatures. [8] An example of the use of the nickel-based superalloys in the industrial field would be turbine blades.
Alloys of nickel are the most common but includes iron aluminum alloys. [1] Applications include high temperature turbine blades and heat exchanger tubing, [2] while steels are used in nuclear applications. [3] ODS materials are used on spacecraft to protect the vehicle, especially during re-entry. Noble metal ODS alloys, for example, platinum ...
Inconel 625 was designed as a solid solution strengthened material with no significant microstructure. This holds true at low and high temperatures, but there is a region (923 to 1148 K) where precipitates form that are detrimental to the creep properties, and thus the strength, of the alloy.