904L is an austenitic stainless steel.It is softer than 316L, [1] [2] and its molybdenum addition gives it superior resistance to localized attack (pitting and crevice corrosion) by chlorides and greater resistance reducing acids; in particular, its copper addition gives it useful corrosion resistance to all concentrations of sulfuric acid.
Strong acids, such as hydrochloric acid and sulfuric acid are common, but different applications use various other acids. Also alkaline solutions can be used for cleaning metal surfaces. Solutions usually also contain additives such as wetting agents and corrosion inhibitors. Pickling is sometimes called acid cleaning if descaling is not needed ...
Alloy 20 is an austenitic stainless steel containing less than 50% iron developed for applications involving sulfuric acid. Its corrosion resistance also finds other uses in the chemical , petrochemical , power generation , and plastics industries.
A typical mixture is 3 parts of concentrated sulfuric acid and 1 part of 30 wt. % hydrogen peroxide solution; [1] other protocols may use a 4:1 or even 7:1 mixture. A closely related mixture, sometimes called "base piranha", is a 5:1:1 mixture of water, ammonia solution ( NH 4 OH , or NH 3 (aq) ), and 30% hydrogen peroxide.
Sulfuric acid is one of the most-produced industrial chemicals. At room temperature, type 304 stainless steel is only resistant to 3% acid, while type 316 is resistant to 3% acid up to 50 °C (120 °F) and 20% acid at room temperature. Thus type 304 SS is rarely used in contact with sulfuric acid.
Electrolytes used for electropolishing are most often concentrated acid solutions such as mixtures of sulfuric acid and phosphoric acid. Other electropolishing electrolytes reported in the literature include mixtures of perchloric acid with acetic anhydride (which has caused fatal explosions), and methanolic solutions of sulfuric acid. [3]
For example, the fracture surface of a fuel connector showed the progressive growth of the crack from acid attack (Ch) to the final cusp (C) of polymer. In this case the failure was caused by hydrolysis of the polymer by contact with sulfuric acid leaking from a car battery. The degradation reaction is the reverse of the synthesis reaction of ...
SAE 316L grade stainless steel, sometimes referred to as A4 stainless steel or marine grade stainless steel, is the second most common austenitic stainless steel after 304/A2 stainless steel. Its primary alloying constituents after iron , are chromium (between 16–18%), nickel (10–12%) and molybdenum (2–3%), up to 2% manganese , [ 1 ] with ...