  2. Conservation and restoration of ceramic objects - Wikipedia

    en.wikipedia.org/wiki/Conservation_and...

    The history of ceramic repair is vast and ranges from different methods and methodologies. For example, in 16th century China, people would repair broken ceramics by using pieces from other objects to disguise the patch. A sixteenth-century manuscript describes the process of patching broken ceramics:

  3. Dropped ceiling - Wikipedia

    en.wikipedia.org/wiki/Dropped_ceiling

    Initially modern dropped ceilings were built using interlocking tiles and the only way to provide access for repair or inspection of the area above the tiles was by starting at the edge of the ceiling, or at a designated "key tile", and then removing contiguous tiles one at a time until the desired place of access was reached.

  4. Kintsugi - Wikipedia

    en.wikipedia.org/wiki/Kintsugi

    Lacquerware is a longstanding tradition in Japan [6] [7] and, at some point, kintsugi may have been combined with maki-e as a replacement for other ceramic repair techniques. . While the process is associated with Japanese craftsmen, the technique was also applied to ceramic pieces of other origins including China, Vietnam, and Kor

  5. AOL Video - Serving the best video content from AOL and ...

    www.aol.com/video/view/how-to-fix-a-loose-tile/...

    The AOL.com video experience serves up the best video content from AOL and around the web, curating informative and entertaining snackable videos.

  6. Glaze defects - Wikipedia

    en.wikipedia.org/wiki/Glaze_defects

    Crazing is a spider web pattern of cracks penetrating the glaze. It is caused by tensile stresses greater than the glaze is able to withstand. [1] [2] Common reasons for such stresses are: a mismatch between the thermal expansions of glaze and body; from moisture expansion of the body; and in the case of glazed tiles fixed to a wall, movement of the wall or of the bonding material used to fix ...

  7. Vitreous enamel - Wikipedia

    en.wikipedia.org/wiki/Vitreous_enamel

    Vitreous enamel, also called porcelain enamel, is a material made by fusing powdered glass to a substrate by firing, usually between 750 and 850 °C (1,380 and 1,560 °F). The powder melts, flows, and then hardens to a smooth, durable vitreous coating.

  8. Conservation and restoration of frescos - Wikipedia

    en.wikipedia.org/wiki/Conservation_and...

    A number of experts criticized the proposed techniques, claiming that the restoration procedure would scrape off the layers of various materials on the frescoes, which would lead to damage beyond repair, and that the removal of the materials would expose the pigments on the frescoes which were fragile and dated to artificial light, temperature ...

  9. Industrial porcelain enamel - Wikipedia

    en.wikipedia.org/wiki/Industrial_porcelain_enamel

    The most important characteristic of porcelain enamel, from an industrial perspective, is its resistance to corrosion. [3] Mild steel is used in almost every industry and a huge array of products; porcelain enamel is a very economic way of protecting this, and other chemically vulnerable materials, from corrosion.