In 1987 the US Department of Agriculture published a method for producing kiln dried firewood, on the basis that better heat output and increased combustion efficiency can be achieved with logs containing lower moisture content. [4] The magazine "Wood Burning Quarterly" was published for several years before changing its name to "Home Energy ...
Firewood with a moisture content below 20 per cent by weight can burn efficiently. This is the "free" moisture content absorbed in the wood fibers, and does not include the chemically-bound hydrogen and oxygen content. Moisture content can be reduced by outdoor air-drying ("seasoning"), for a period of several months in summer weather.
The energy content of a measure of wood depends on the tree species. [19] For example, it can range from 15.5 to 32 million British thermal units per cord (4.5 to 9.3 GJ/m 3). [20] The higher the moisture content, the more energy that must be used to evaporate (boil) the water in the wood before it will burn. Dry wood delivers more energy for ...
The burning of wood results in about 6–10% ashes on average. [2] The residue ash of 0.43 and 1.82 percent of the original mass of burned wood (assuming dry basis, meaning that H 2 O is driven off) is produced for certain woods if it is pyrolized until all volatiles disappear and it is burned at 350 °C (662 °F) for 8 hours.
Wood in this process must have a moisture content at 12% or lower which can be attained through simple drying processes. The wood is then placed in a high nitrogen atmosphere with no more than 2% oxygen content. [8] The Perdure Process is relatively similar to retification but holds the wood at a lower temperature. [9]
Cord wood generally needs to be "seasoned" or "dry" before it can be burned cleanly and efficiently. On the other hand, woodchip systems are typically designed to cleanly and efficiently burn "green chips" with very high moisture content of 43–47% (wet basis). [13] (see gasification and woodgas)
The chemical potential of sorbed water is a function of wood moisture content. Therefore, a gradient of wood moisture content (between surface and centre), or more specifically of water activity, is accompanied by a gradient of chemical potential under isothermal conditions. Moisture will redistribute itself throughout the wood until its ...
Equilibrium moisture content in wood. In heartwood it occurs only in the first and last forms. Wood that is thoroughly air-dried (in equilibrium with the moisture content of the air) retains 8–16% of the water in the cell walls, and none, or practically none, in the other forms. Even oven-dried wood retains a small percentage of moisture, but ...