Wood drying (also seasoning lumber or wood seasoning) reduces the moisture content of wood before its use. When the drying is done in a kiln , the product is known as kiln-dried timber or lumber , whereas air drying is the more traditional method.
Wood in this process must have a moisture content at 12% or lower which can be attained through simple drying processes. The wood is then placed in a high nitrogen atmosphere with no more than 2% oxygen content. [8] The Perdure Process is relatively similar to retification but holds the wood at a lower temperature. [9]
In North America, logs reach equilibrium moisture content at about 6% and 12%; [8] since most kiln-dried logs are dried down to about 18% to 20% moisture content, kiln-dried logs can be expected to shrink and settle over time, but to a lesser extent than green logs.
The moisture content of firewood determines how it burns and how much heat is released. Unseasoned (green) wood moisture content varies by the species; green wood may weigh 70 to 100 percent more than seasoned wood due to water content. Typically, seasoned (dry) wood has 20% or less moisture content. Use of the lower heating value is advised as ...
Further drying of the wood results in strengthening of the wood fibres, [1] and is usually accompanied by shrinkage. Wood is normally dried to a point where it is in equilibrium with the atmospheric moisture content or relative humidity, and since this varies so does the equilibrium moisture content. Laboratory testing has found the average FSP ...
Green wood coming straight from the felled tree has far too high a moisture content to be commercially useful and will rot, warp and split. Both hardwoods and softwood must be left to dry out until the moisture content is between 18% and 8%. This can be a long process unless accelerated by use of a kiln.
Green wood is considered to have 100% moisture content relative to air-dried or seasoned wood, which is considered to be 20%. Energy density charts for wood fuels tend to use air dried wood as their reference, thus oven dried or 0% moisture content can reflect 103.4% energy content.
The wood moisture content is above 25% on a dry-weight basis; The environment is sufficiently warm; Oxygen (O 2) is present; Wood with less than 25% moisture (dry weight basis) can remain free of decay for centuries. Similarly, wood submerged in water may not be attacked by fungi if the amount of oxygen is inadequate. Fungi lumber/timber ...