Search results
Results from the WOW.Com Content Network
Microstructures of four kinds of duplex stainless steel in each direction. Duplex stainless steels are usually divided into three groups based on their pitting corrosion resistance, characterised by the pitting resistance equivalence number, PREN = %Cr + 3.3 %Mo + 16 %N.
Pitting resistance equivalent number (PREN) is a predictive measurement of a stainless steel's resistance to localized pitting corrosion based on its chemical composition. In general: the higher PREN-value, the more resistant is the stainless steel to localized pitting corrosion by chloride.
SAF 2205, is a Alleima-owned trademark (Formerly Sandvik Materials Technology) for a 22Cr duplex (ferritic-austenitic) stainless steel. SAF derives from Sandvik Austenite Ferrite.
904L is an austenitic stainless steel.It is softer than 316L, [1] [2] and its molybdenum addition gives it superior resistance to localized attack (pitting and crevice corrosion) by chlorides and greater resistance reducing acids; in particular, its copper addition gives it useful corrosion resistance to all concentrations of sulfuric acid.
Convergent beam electron diffraction (CBED) transmission electron micrograph of a [111] zone axis of austenitic stainless steel. Austenitic stainless steel is one of the five families of stainless steel (along with ferritic, martensitic, duplex and precipitation hardened). [1]
Crevice corrosion of 316 stainless steel from desalination.. SAE 316L grade stainless steel, sometimes referred to as A4 stainless steel or marine grade stainless steel, is the second most common austenitic stainless steel after 304/A2 stainless steel.
Marine grade stainless alloys typically contain molybdenum to resist the corrosive effects of NaCl or salt in seawater. Concentrations of salt in seawater can vary, and splash zones can cause concentrations to increase dramatically from the spray and evaporation.
Thermal conductivities have been measured with longitudinal heat flow methods where the experimental arrangement is so designed to accommodate heat flow in only the axial direction, temperatures are constant, and radial heat loss is prevented or minimized.