Carbon content has a strong influence on room temperature strength and thus the specified minimum tensile properties of 304L are 34 MPa (5,000 psi) lower than for 304. However, nitrogen also has a strong influence on room temperature strength and a tiny addition of nitrogen produces 304L with the same tensile strength as 304.
It can be strengthened by cold working to a strength of 1,050 MPa (153,000 psi) in the full-hard condition. The strongest commonly available stainless steels are precipitation hardening alloys such as 17-4 PH and Custom 465. These can be heat treated to have tensile yield strengths up to 1,730 MPa (251,000 psi). [8]
Specified Minimum Yield Strength (SMYS) means the specified minimum yield strength for steel pipe manufactured in accordance with a listed specification 1. This is a common term used in the oil and gas industry for steel pipe used under the jurisdiction of the United States Department of Transportation .
In one study, strain hardening exponent values extracted from tensile data from 58 steel pipes from natural gas pipelines were found to range from 0.08 to 0.25, [1] with the lower end of the range dominated by high-strength low alloy steels and the upper end of the range mostly normalized steels.
Duplex steels also have higher strength. For example, a Type 304 stainless steel has a 0.2% proof strength in the region of 280 MPa (41 ksi), a 22%Cr duplex stainless steel a minimum 0.2% proof strength of some 450 MPa (65 ksi) and a superduplex grade a minimum of 550 MPa (80 ksi). [6]
For ductile materials, the yield strength is typically distinct from the ultimate tensile strength, which is the load-bearing capacity for a given material. The ratio of yield strength to ultimate tensile strength is an important parameter for applications such steel for pipelines , and has been found to be proportional to the strain hardening ...
Due to the power-law relationship between stress and plastic strain, the Ramberg–Osgood model implies that plastic strain is present even for very low levels of stress. Nevertheless, for low applied stresses and for the commonly used values of the material constants α {\displaystyle \alpha } and n {\displaystyle n} , the plastic strain ...
Type 316LN—same as 316L with nitrogen added to obtain a higher yield and tensile strength than 316L. Type 316Ti—variant of type 316 that includes titanium for heat resistance. It is used in flexible chimney liners. Type 317 [8] Type 321—similar to 304 but lower risk of weld decay due to addition of titanium.