CPP and CPR methods, developed over the last 40 years, are used in lieu of asphalt overlays and bituminous patches to repair roads when longer lasting solutions are desired. When installing pavers over top of an existing asphalt of concrete pad, there are three installation options: sand set, bituminous set, and mortar set. [1]
BS 1881:204 Testing concrete. Recommendations on the use of electromagnetic covermeters; DGZfP:B2: Guideline “für Bewehrungsnachweis und Überdeckungsmessung bei Stahl- und Spannbeton” DIN 1045: Guideline Concrete, reinforced and prestressed concrete structures; ACI Concrete Practices Non Destructive testing 228.2R-2.51: Covermeters
A falling weight deflectometer (FWD) is a testing device used by civil engineers to evaluate the physical properties of pavement in highways, local roads, airport pavements, harbor areas, railway tracks and elsewhere. The data acquired from FWDs is primarily used to estimate pavement structural capacity, to facilitate overlay design or ...
The test method for conducting the test usually involves a specified test fixture on a universal testing machine. Details of the test preparation, conditioning, and conduct affect the test results. The sample is placed on two supporting pins a set distance apart and two loading pins placed at an equal distance around the center.
The anchor selection, together with additional reinforcement, and rigging arrangements is influenced by: - The dead weight of the element - The number of anchors in the element and the configuration of the anchor - Capacity of the anchor at the specific concrete compressive strengths at time of lift - The dynamic loads applied during lifting ...
The test is carried out using a metal mould in the shape of a conical frustum known as a slump cone or Abrams cone, that is open at both ends and has attached handles.The tool typically has an internal diameter of 100 millimetres (3.9 in) at the top and of 200 millimetres (7.9 in) at the bottom with a height of 305 millimetres (12.0 in).The cone is placed on a hard non-absorbent surface.
The test hammer hits the concrete at a defined energy. Its rebound is dependent on the hardness of the concrete and is measured by the test equipment. By reference to a conversion chart, the rebound value can be used to determine the concrete's compressive strength. When conducting the test, the hammer should be held at right angles to the ...
The test reports loss of mass to abrasion and impact, expressed as a percentage of initial sample mass. [7] Maximum acceptable loss for the base course of the road is 45%; the more demanding surface course must be 35% or less. [1] The test was developed by the city engineers of Los Angeles in the 1920s. [8]