enow.com Web Search

Search results

  1. Results from the WOW.Com Content Network
  2. Basement waterproofing - Wikipedia

    en.wikipedia.org/wiki/Basement_waterproofing

    Buckling walls: Usually caused by hydrostatic pressure. Walls appear to be bowed inward. Peeling paint: Water seeping through walls may lead to bubbling or peeling paint along basement walls. [4] Efflorescence: White, powdery residue found on basement walls near the floor.

  3. Efflorescence - Wikipedia

    en.wikipedia.org/wiki/Efflorescence

    Primary efflorescence is named such, as it typically occurs during the initial cure of a cementitious product. It often occurs on masonry construction, particularly brick, as well as some firestop mortars, when water moving through a wall or other structure, or water being driven out as a result of the heat of hydration as cement stone is being formed, brings salts to the surface that are not ...

  4. Concrete degradation - Wikipedia

    en.wikipedia.org/wiki/Concrete_degradation

    Example of flat piece of concrete having dislodged with corroded rebar underneath, Welland River bridge across Queen Elizabeth Way in Niagara Falls, Ontario. The expansion of the corrosion products (iron oxides) of carbon steel reinforcement structures may induce internal mechanical stress (tensile stress) that cause the formation of cracks and disrupt the concrete structure.

  5. Concrete block - Wikipedia

    en.wikipedia.org/wiki/Concrete_block

    A pallet of "8-inch" concrete blocks An interior wall of painted concrete blocks Concrete masonry blocks A building constructed with concrete masonry blocks. A concrete block, also known as a cinder block in North American English, breeze block in British English, concrete masonry unit (CMU), or by various other terms, is a standard-size rectangular block used in building construction.

  6. Sulfate attack in concrete and mortar - Wikipedia

    en.wikipedia.org/wiki/Sulfate_attack_in_concrete...

    When it reacts with concrete, it causes the slab to expand, lifting, distorting and cracking as well as exerting a pressure onto the surrounding walls which can cause movements significantly weakening the structure. Some infill materials frequently encountered in building fondations and causing sulfate attack are the following: [2] Red Ash

  7. Alkali–silica reaction - Wikipedia

    en.wikipedia.org/wiki/Alkali–silica_reaction

    ASTM C1293: "Test Method for Concrete Aggregates by Determination of Length Change of Concrete Due to Alkali-Silica Reaction". It is a long-term confirmation test (1 or 2 years) at 38 °C in a water-saturated moist atmosphere (inside a thermostated oven) with concrete prisms containing the aggregates to be characterised mixed with a high-alkali ...

  8. Properties of concrete - Wikipedia

    en.wikipedia.org/wiki/Properties_of_concrete

    The ultimate strength of concrete is influenced by the water-cementitious ratio (w/cm), the design constituents, and the mixing, placement and curing methods employed.All things being equal, concrete with a lower water-cement (cementitious) ratio makes a stronger concrete than that with a higher ratio. [2]

  9. Infill wall - Wikipedia

    en.wikipedia.org/wiki/Infill_wall

    The infill wall is the supported wall that closes the perimeter of a building constructed with a three-dimensional framework structure (generally made of steel or reinforced concrete). Therefore, the structural frame ensures the bearing function, whereas the infill wall serves to separate inner and outer space, filling up the boxes of the outer ...