The Janka hardness test (English: / ˈ dʒ æ ŋ k ə /; [1] German:), created by Austrian-born American researcher Gabriel Janka (1864–1932), measures the resistance of a sample of wood to denting and wear. [citation needed] It measures the force required to embed an 11.28-millimeter-diameter (7 ⁄ 16 in) steel ball halfway into a sample of ...
The native North American wood variety has a subtle grain with a tendency to darken and yellow more over an extended period of time. It's highly durable and measures 1450 on the Janka scale.
Lignum vitae is hard and durable, and is also the densest wood traded (average dried density: ~79 lb/ft 3 or ~1,260 kg/m 3); [4] it will easily sink in water. On the Janka scale of hardness, which measures hardness of woods, lignum vitae ranks highest of the trade woods, with a Janka hardness of 4,390 lbf (compared with Olneya at 3,260 lbf, [5] African blackwood at 2,940 lbf, hickory at 1,820 ...
The wood is extremely hard, being one of the hardest woods in Northern America with a Janka hardness test of 1,700 lbf (7,560 N) [46] and specific gravity of 0.733 (733 kilograms per cubic metre or 45.7 pounds per cubic foot).
Both kinds of wood are hard (with a Janka hardness of 550 lbf (2,400 N)), but the western yellow pine wood is less dense than southern yellow pine wood (28 lb/cu ft (0.45 g/cm 3) versus 35 lb/cu ft (0.56 g/cm 3) for shortleaf pine).
Hardness Conversion Table – Brinell, Rockwell,Vickers – Various steels . (archived November 11, 2011) Rockwell to Brinell conversion chart (Brinell, Rockwell A,B,C) Struers hardness conversion table (Vickers, Brinell, Rockwell B,C,D)
The Brinell scale; The Janka hardness test; The Rockwell scale; The Durometer scale; The Barcol scale; The Leeb rebound hardness scale; The Rosiwal scale; The Meyer ...
Both kinds of wood are hard (with a Janka hardness of 550 lbf (2,400 N)), but the western yellow pine wood is less dense than southern yellow pine wood (28 lb/cu ft (0.45 g/cm 3) versus 35 lb/cu ft (0.56 g/cm 3) for shortleaf pine). [10]