In the recent past, HSS was commonly available in mild steel, such as A500 grade B. Today, HSS is commonly available in mild steel, A500 grade C. Other steel grades available for HSS are A847 (weathering steel), A1065 (large sections up to 50 inch sq made with SAW process), and recently approved A1085 (higher strength, tighter tolerances than ...
High-speed steel (HSS or HS) is a subset of tool steels, commonly used as cutting tool material. It is superior to high-carbon steel tools in that it can withstand higher temperatures without losing its temper (hardness). This property allows HSS to cut faster than high carbon steel, hence the name high-speed steel.
With the stronger HY-80 steel, this depth increased to 1,800 feet (550 m) and with HY-100 a depth of 2,250 feet (690 m). [2] The first production submarines to use HY-80 steel were the Permit class. These reportedly had a normal operating depth of 1,300 feet, roughly two-thirds the crush depth limit imposed by the steel. [2]
The weight of a rail per length is an important factor in determining rail strength and hence axleloads and speeds. Weights are measured in pounds per yard (imperial units in Canada, the United Kingdom and United States) and kilograms per metre in mainland Europe and Australia). 1 kg/m = 2.0159 lb/yd.
ASTM A992 steel is a structural steel alloy often used in the US for steel wide-flange and I beams. Like other carbon steels, the density of ASTM A992 steel is approximately 7850 kg/m 3 (0.2836 lb/in 3). ASTM A992 steel has the following minimum mechanical properties, according to ASTM specification A992/A992M.
ASTM A500 is a standard specification published by the ASTM for cold-formed welded and seamless carbon steel structural tubing in round, square, and rectangular shapes. It is commonly specified in the US for hollow structural sections, but the more stringent CSA G40.21 is preferred in Canada.
A36 steel has a Poisson's ratio of 0.26 and a shear modulus of 11,500 ksi (79.3 GPa). [ 7 ] A36 steel in plates, bars, and shapes with a thickness of less than 8 inches (203 millimeters) has a minimum yield strength of 36 ksi (250 MPa ) and ultimate tensile strength of 58–80 ksi (400–550 MPa).
A tungsten carbide tipped (TCT) and high-speed steel (HSS) annular cutter (also known as a "core drill" or "hole saw"). An annular cutter (also called a core drill, core cutter, broach cutter, trepanning drill, hole saw, or cup-type cutter) is a form of core drill used to create holes in metal.