Shotcrete is placed and compacted/consolidated at the same time, due to the force with which it is ejected from the nozzle. It can be sprayed onto any type or shape of surface, including vertical or overhead areas. Shotcrete has the characteristics of high compressive strength, good durability, water tightness and frost resistance. [2]
High-strength concrete has a compressive strength greater than 40 MPa (6000 psi). In the UK, BS EN 206-1 [3] defines High strength concrete as concrete with a compressive strength class higher than C50/60. High-strength concrete is made by lowering the water-cement (W/C) ratio to 0.35 or lower.
Traditional rebars are generally used to improve the tensile strength of the concrete in a particular direction, whereas steel fibers are useful for multidirectional reinforcement. This is one of the reasons why steel fiber reinforced (shotcrete form) concrete successfully replaced weldmesh in lining tunnels. Less labour is required.
The early strength of the concrete can be increased if it is kept damp during the curing process. Minimizing stress prior to curing minimizes cracking. High-early-strength concrete is designed to hydrate faster, often by increased use of cement that increases shrinkage and cracking. The strength of concrete changes (increases) for up to three ...
Twenty eight days is a long wait to determine if desired strengths are going to be obtained, so three-day and seven-day strengths can be useful to predict the ultimate 28-day compressive strength of the concrete. A 25% strength gain between 7 and 28 days is often observed with 100% OPC (ordinary Portland cement) mixtures, and between 25% and 40 ...
The test hammer hits the concrete at a defined energy. Its rebound is dependent on the hardness of the concrete and is measured by the test equipment. By reference to a conversion chart, the rebound value can be used to determine the concrete's compressive strength. When conducting the test, the hammer should be held at right angles to the ...
Concrete spalling from the ceiling of an office unit (interior) in Singapore, possibly due to rebar corrosion. Reinforced concrete can fail due to inadequate strength, leading to mechanical failure, or due to a reduction in its durability. Corrosion and freeze/thaw cycles may damage poorly designed or constructed reinforced concrete.
A higher porosity reduces the final strength of concrete because the air present in the pores is compressible and concrete microstructure can be more easily "crushed". Moreover, a higher porosity also increases the hydraulic conductivity ( K , m/s) of concrete and the effective diffusion coefficients ( D e , m 2 /s) of solutes and dissolved ...
Ad