Manganin is a trademarked name for an alloy of typically 84.2% copper, 12.1% manganese, and 3.7% nickel. It was first developed by Edward Weston in 1892, improving upon his Constantan (1887). Manganin foil and wire is used in the manufacture of resistors , particularly ammeter shunts , because of its virtually zero temperature coefficient of ...
This is a list of named alloys grouped alphabetically by the metal with the highest percentage. Within these headings, the alloys are also grouped alphabetically. Within these headings, the alloys are also grouped alphabetically.
Other constant-resistance alloys include manganin (Cu 86 Mn 12 Ni 2), Cupron (Cu 53 Ni 44 Mn 3) [2] and Evanohm. Melts at about 1,220 °C (2,230 °F). Melts at about 1,220 °C (2,230 °F). Balco ( Ni 70 Fe 30 ) and similar alloys have very high, but more linear, temperature coefficients of resistivity, making them suitable for sensing elements.
Copper alloys of manganese, such as Manganin, are commonly found in metal element shunt resistors used for measuring relatively large amounts of current. These alloys have very low temperature coefficient of resistance and are resistant to sulfur. This makes the alloys particularly useful in harsh automotive and industrial environments. [83]
Very importantly, constantan can be processed for self-temperature compensation to match a wide range of test material coefficients of thermal expansion.A-alloy is supplied in self-temperature-compensation (S-T-C) numbers 00, 03, 05, 06, 09, 13, 15, 18, 30, 40, and 50, for use on test materials with corresponding thermal expansion coefficients, expressed in parts per million by length (or μm ...
A typical shunt consists of two solid metal blocks, sometimes brass, mounted on an insulating base. Between the blocks, and soldered or brazed to them, are one or more strips of low temperature coefficient of resistance (TCR) manganin alloy. Large bolts threaded into the blocks make the current connections, while much smaller screws provide ...
For manganin, a common shunt material, at 80 °C thermal drift begins to occur, at 120 °C thermal drift is a significant problem where error, depending on the design of the shunt, can be several percent and at 140 °C the manganin alloy becomes permanently damaged due to annealing resulting in the resistance value drifting up or down.
The invention of "Manganin," the alloy now used universally for resistors of high accuracy, followed shortly thereafter. The resistance of "Manganin" is virtually constant within reasonable temperature limits. 1888 The Weston Electrical Instrument Co. is formed by Edward Weston. Dr.