Hot gas welding, also known as hot air welding, is a plastic welding technique using heat. A specially designed heat gun, called a hot air welder, produces a jet of hot air that softens both the parts to be joined and a plastic filler rod, all of which must be of the same or a very similar plastic. (Welding PVC to acrylic is an exception to ...
When the welding direction is parallel to the orientation of the fibers, the weld width is usually narrower due to heat being channeled through the fibers to the front and the rear of the weld. [ 6 ] Increased volume fraction of reinforcements such as glass can scatter the laser beam, thus allowing less to be transmitted to the weld joint.
Spin welding creates a clean and sound weld joint that requires little post processing. [3] Due to this most parts being welded are in the final stages of production, or are in final assembly. The first known application of spin welding was in the assembly of compasses, however spin welding has become used in a wide variety of products.
During laser welding, air bubbles can form and cause a degradation in the mechanical properties of the joint. Current inspection techniques are limited to finding air bubbles on the surface of the weld (optical and scanning electron microscopy). Destructive testing is usually required to find volumetric flaws.
Solvent bonding differs from other plastic welding processes in that heating energy is generated by the chemical reaction between the solvent and thermoplastic, and cooling occurs during evaporation of the solvent. [5] Solvent bonding can be performed using a liquid or gaseous solvent.
The main obstacle to overcome in this process is the setting of the parameters. For example, if over-welding occurs, then the concentration of plastic in the weld zone may be too low and cause the seal to break. If it is under-welded, the seal is incomplete. [17] Variations in the thicknesses of materials can cause variations in weld quality.