Nimonic alloys typically consist of more than 50% nickel and 20% chromium with additives such as titanium and aluminium. The main use is in gas turbine components and extremely high performance reciprocating internal combustion engines.
Print/export Download as PDF; ... Nickel alloys are alloys with nickel as principal element. ... This list may not reflect recent changes. A. AL-6XN;
The next family of Co-based superalloys was discovered in 2015 by Makineni et al. This family has a similar γ/γ' microstructure, but is W-free and has a γ' phase of Co 3 (Al,Mo,Nb). [16] Since W is heavy, its elimination makes Co-based alloys increasingly viable in turbines for aircraft, where low density is especially valued.
Originally developed to produce oxide-dispersion strengthened (ODS) nickel- and iron-base superalloys for applications in the aerospace industry, [1] MA has now been shown to be capable of synthesizing a variety of equilibrium and non-equilibrium alloy phases starting from blended elemental or pre-alloyed powders. [2]
Inconel is a nickel-chromium-based superalloy often utilized in extreme environments where components are subjected to high temperature, pressure or mechanical loads. Inconel alloys are oxidation- and corrosion-resistant. When heated, Inconel forms a thick, stable, passivating oxide layer protecting the surface from further attack.
In nickel-based superalloys, regions of Ni 3 Al (called γ' phase) precipitate out of the nickel-rich matrix (called γ phase) to give high strength and creep resistance. Many alloy formulations are available and they usually include other elements, such as chromium, molybdenum, and iron, in order to improve various properties.
Alloys of nickel are the most common but includes iron aluminum alloys. [1] Applications include high temperature turbine blades and heat exchanger tubing, [2] while steels are used in nuclear applications. [3] ODS materials are used on spacecraft to protect the vehicle, especially during re-entry. Noble metal ODS alloys, for example, platinum ...
Directional solidification is the preferred technique for casting high temperature nickel-based superalloys that are used in turbine engines of aircraft. Some microstructural problems such as coarse dendritic structure, long dendrite side branches, and porosity hinder the full potential of single crystal ni-based alloys. [ 6 ]