    Increasing the temperature of the material or mold allows the material to flow without stiffening before the cycle completes. [ 1 ] If the temperature is increased too high, there is a chance to cause a different type of injection molding defect referred to as a burn mark .

  3. Injection moulding - Wikipedia

    en.wikipedia.org/wiki/Injection_moulding

    Injection moulding (U.S. spelling: injection molding) is a manufacturing process for producing parts by injecting molten material into a mould, or mold. Injection moulding can be performed with a host of materials mainly including metals (for which the process is called die-casting ), glasses , elastomers , confections , and most commonly ...

  4. Weld line - Wikipedia

    en.wikipedia.org/wiki/Weld_line

    In manufacturing, the Weld line or Knit line or Meld line is the line where two flow fronts meet when there is the inability of two or more flow fronts to "knit" together, or "weld", during the molding process. These lines usually occur around holes or obstructions and cause locally weak areas in the molded part. [1]

  5. Injection molding of liquid silicone rubber - Wikipedia

    en.wikipedia.org/wiki/Injection_molding_of...

    Injection molding of liquid silicone rubber (LSR) is a process to produce pliable, durable parts in high volume.. Liquid silicone rubber is a high purity platinum cured silicone with low compression set, good stability and ability to resist extreme temperatures of heat and cold ideally suitable for production of parts, where high quality is required.

  6. Splay (plastics) - Wikipedia

    en.wikipedia.org/wiki/Splay_(plastics)

    The moisture turns to steam when heated in the barrel of the machine, and becomes tiny gas bubbles that streak across the plastic as injection occurs. [2] This causes the silvery pattern, or streaks, to appear on the surface of the plastic. Splay can be avoided by keeping moisture out of plastics and injection molding machines.

  7. Trump Adviser Alex Bruesewitz, 27, Collapses on Stage at N.Y ...

    www.aol.com/trump-adviser-alex-bruesewitz-27...

    Donald Trump campaign adviser Alex Bruesewitz collapsed on stage during an appearance at a Republican event in New York City.. On Sunday, Dec. 15, the 27-year-old political strategist was ...

  8. Lobby group asks Trump for investment rules overhaul - AOL

    www.aol.com/news/lobby-group-asks-trump...

    A trade group has asked the incoming Trump administration to consider a "comprehensive plan" for updating the U.S. Securities and Exchange Commission's regulatory framework for investment ...

  9. Flash (manufacturing) - Wikipedia

    en.wikipedia.org/wiki/Flash_(manufacturing)

    In plastic injection, a faint mark called a witness mark (or witness line) will occur along the parting line. [1] This is unavoidable and is usually accepted despite the minor aesthetics issue. However, some part surfaces (e.g. when used for sealing [ 5 ] ) cannot tolerate witness marks, and thus either the marks must be removed post-molding or ...