enow.com Web Search

Search results

  1. Results from the WOW.Com Content Network
  2. Undercut (welding) - Wikipedia

    en.wikipedia.org/wiki/Undercut_(welding)

    Undercut created during welding. In welding, undercutting is when the weld reduces the cross-sectional thickness of the base metal. This type of defect reduces the strength of the weld and workpieces.

  3. Weld quality assurance - Wikipedia

    en.wikipedia.org/wiki/Weld_quality_assurance

    Methods of weld testing and analysis are used to assure the quality and correctness of the weld after it is completed. This term generally refers to testing and analysis focused on the quality and strength of the weld but may refer to technological actions to check for the presence, position, and extent of welds.

  4. Symbols and conventions used in welding documentation

    en.wikipedia.org/wiki/Symbols_and_conventions...

    The symbolic representation of a V weld of chamfered plates in a technical drawing. The symbols and conventions used in welding documentation are specified in national and international standards such as ISO 2553 Welded, brazed and soldered joints -- Symbolic representation on drawings and ISO 4063 Welding and allied processes -- Nomenclature of processes and reference numbers.

  5. Engineering Critical Assessment - Wikipedia

    en.wikipedia.org/wiki/Engineering_Critical...

    Engineering Critical Assessment (ECA) is a procedure by which the safety of a welded structure with defects or flaws can be determined. ECAs utilize the material properties and expected stress history to determine a flaw acceptance criteria which will ensure that welds will not fail during the construction or service life of the welded structure. [1]

  6. Welding defect - Wikipedia

    en.wikipedia.org/wiki/Welding_defect

    Cold cracking—also known as delayed cracking, hydrogen-assisted cracking (HAC), or hydrogen-induced cracking (HIC)—is a type of defect that often develops after solidification of the weld when the temperature starts to drop from about 190 °C (375 °F); the phenomenon often arises at room temperature, and it can take up to 24 hours to appear even after complete cooling. [8]

  7. 51 'Mr. Everymans' were found guilty of rape. How Gisele ...

    www.aol.com/news/51-mr-everymans-were-found...

    The French rape trial that shocked the world and sparked widespread calls for justice for women rape victims ended on Thursday with the conviction of 51 men for raping and attempting to rape ...

  8. List of welding codes - Wikipedia

    en.wikipedia.org/wiki/List_of_welding_codes

    Covered electrodes for manual metal arc welding of non-alloy and fine grain steels. Classification ISO 3580: Covered electrodes for manual arc welding of creep-resisting steels - Code of symbols for identification ISO 3581: Covered electrodes for manual arc welding of stainless and other similar high alloy steels - Code of symbols for ...

  9. ‘Like going to the moon’: Why this is the world’s most ...

    www.aol.com/going-moon-why-world-most-120326810.html

    Navigating the Drake is an extremely complex task that demands humility and a side of fear, says Captain Stanislas Devorsine, one of three captains of Le Commandant Charcot, a polar vessel of ...